Technical data
Outer laminate: DuPont™ Mylar®
| Electrical properties | |||
| Properties of the base film | Typical value | Test condition | Test method |
| 37.5 HS Slide (37 μm) | |||
| dielectric strength) [kV] | > 3,5 | ASTM D 149 | |
| Physical properties | ||||
| Properties of the base film | Typical value | Test condition | Test method | |
| 37.5 HS Slide (37 μm) | ||||
| Tear resistance | ||||
| LR
QR |
[Mpa] | 190 | Running direction (LR) | ASTM D 882 |
| 260 | Transverse direction (QR) | ASTM D 882 | ||
| Yield [m2/kg] | 19,10 | |||
| Tension module | ||||
| LR
QR |
[Mpa] | 2,100 | LR | ASTM D 882 |
| 3,600 | QR | ASTM D 882 | ||
| Yield point | ||||
| LR
QR |
[%] | 170 | LR | ASTM D 882 |
| 110 | QR | ASTM D 882 | ||
| Water vapor permeability | [g/m2/24 h] | 15 | 38°C, 90% relative humidity | ASTM F 1249 |
| Oxygen permeability | [cm3/m2/24 h] | 75 | before shrinking | ASTM D 3985 |
| 30-45 | after shrinking | ASTM D 3985 | ||
| Optical properties | ||
| Properties of the base film | Typical value | Test method |
| Melting point | 253-255°C (526-528 K) | ASTM D 3148-82 |
Inner laminate: DuPont™ Nomex® Grade 411
| Electrical properties | ||||
| Properties of the film | Film thickness | Test condition | Test method | |
| 0.130 mm | 0.180 mm | |||
| Dielectric strength [kV/mm] | 12 | 12 | AC steep ascent | ASTM D 149 |
| Dielectric constant | 1,3 | 1,3 | 1000 Hz | ASTM D 150 |
| Loss factor | 0,005 | 0,005 | 1000 Hz | ASTM D 150 |
| Physical properties | ||||
| Properties of the film | Typical value | Test condition | Test method | |
| Tear resistance | ||||
| LR QR | [N/cm] | 17 | 28 | ASTM D 828-60 |
| 9 | 17 | ASTM D 828-60 | ||
| Elongation | ||||
| LR
QR |
[%] | 3,5 | 3,5 | ASTM D 828-60 |
| 4,8 | 5 | ASTM D 828-60 | ||